铜陵电厂凝汽器黄铜管换不锈钢管
[align=center]梁 磊1 ,周国定1 ,倪 鹏2 ,张登云2 ,孙志林2 ,孙 军2 ,王义好2(1 上海电力学院,上海200090 ;2 安徽铜陵发电厂,安徽铜陵244012)[/align]
摘要:经过多方面的调查、试验和研究,铜陵电厂将1 号机凝汽器HSn70 - 1 黄铜管全部换成了304 不锈钢管,与黄铜管相比,不锈钢管具有较好的耐蚀性能、机械性能、经济性能, ,总的传热性能也不差,取得了较好的效果。
关键词:凝汽器;不锈钢管;黄铜管
分类号: TK265 文献标识码:A
文章编号:100125884 (2004) 0420305203
[align=center]Application of Stainless Steel Tubes for Condenser in Tongling
Power Plant Instead of Brass Tubes[/align]
[align=center]LIANGLei1 ,ZHOU Guo2ding1 ,NI Peng2 ,ZHANGDeng2yun2 ,SUN Zhi2lin2 ,SUN Jun2 ,WANG Yi2hao2
(1 Shanghai University of Elect ric Power ,Shanghai 200090 ,China ;
2 Tongling Power Plant ,Anhui Tongling 244012 ,China ;)[/align]
Abstract :Stainless steel tubes have been used instead of brass tubes for condenser in Tongling Power Plant after investiga2
tion , research and test . The corrosion2resistance , mechanical strength and economics of stainless steel tubes are better
than brass tubes. The general heat transfer performance of the stainless steel tube condenser is comparable with the brass
tube condenser.
Key words :condenser ;stainless steel tube ;brass tube
0 前 言
铜陵电厂1 号机功率为125MW ,1989 年建成投产。凝汽器型号为N - 7100 - Ⅲ,装有<25 ×1. 0 ×7 565 HSn70 - 1黄铜管12 076根。新铜管使用不到4 个月,就发生了腐蚀泄漏。1994 年和1997 年因为黄铜管腐蚀泄漏较多,两次更换黄铜管。每次更换一半,更换的管子仍为HSn70 - 1 黄铜管。至2002 年大修前,又因为黄铜管腐蚀泄漏较多,需要更换全部凝汽器管。铜陵电厂与上海电力学院合作,经过多方面的调查、试验和研究,从选材、订货、检验、安装和运行等各个环节把好关,在未改动管板、未增加管子根数、使用原循环水泵的条件下,于2002 年10 月大修时将HSn70 - 1 黄铜管全部换成了304 不锈钢管,取得了较好的效果。
......